<< Chapter < Page Chapter >> Page >

This module was developed as part of the Rice University course CHEM-496: Chemistry of Electronic Materials . This module was prepared with the assistance of Julie A. Francis.

Introduction

The growth of thin films has had dramatic impact on technological progress. Because of the various properties and functions of these films, their applications are limitless especially in microelectronics. These layers can act as superconductors, semiconductors, conductors, insulators, dielectric, or ferroelectrics. In semiconductor devices, these layers can act as active layers and dielectric, conducting, or ion barrier layers. Depending on the type of film material and its applications, various deposition techniques may be employed. For gas-phase deposition, these include vacuum evaporation, reactive sputtering, chemical vapor deposition (CVD), especially metal organic CVD (MOCVD), and molecular beam epitaxy (MBE). Atomic layer deposition (ALD), originally called atomic layer epitaxy (ALE), was first reported by Suntola et al. in 1980 for the growth of zinc sulfide thin films to fabricate electroluminescent flat panel displays.

ALD refers to the method whereby film growth occurs by exposing the substrate to its starting materials alternately. It should be noted that ALE is actually a sub-set of ALD, in which the grown film is epitaxial to the substrate; however, the terms are often used interchangeably. Although both ALD and CVD use chemical (molecular) precursors, the difference between the techniques is that the former uses self limiting chemical reactions to control in a very accurate way the thickness and composition of the film deposited. In this regard ALD can be considered as taking the best of CVD (the use of molecular precursors and atmospheric or low pressure) and MBE (atom-by-atom growth and a high control over film thickness) and combining them in single method. A selection of materials deposited by ALD is given in [link] .

Examples of thin film materials deposited by ALD including films deposited in epitaxial, polycrystalline or amorphous form. Adapted from M. Ritala and M. Leskel, Nanotechnology , 1999, 10 , 19.
Compound class Examples
II–VI compounds ZnS, ZnSe, ZnTe, ZnS 1−x Se x , CaS, SrS, BaS, SrS 1−x Se x , CdS, CdTe, MnTe, HgTe, Hg 1−x Cd x Te, Cd 1−x Mn x Te
II–VI based thin-film electroluminescent (TFEL) phosphors ZnS:M (M = Mn, Tb, Tm), CaS:M (M = Eu, Ce, Tb, Pb), SrS:M (M = Ce, Tb, Pb, Mn, Cu)
III–V compounds GaAs, AlAs, AlP, InP, GaP, InAs, Al x Ga 1−x As, Ga x In 1−x As, Ga x In 1−x P
Semiconductors/dielectric nitrides AlN, GaN, InN, SiN x
Metallic nitrides TiN, TaN, Ta 3 N 5 , NbN, MoN
Dielectric oxides Al 2 O 3 , TiO 2 , ZrO 2 , HfO 2 , Ta 2 O 5 , Nb 2 O 5 , Y 2 O 3 , MgO, CeO 2 , SiO 2 , La 2 O 3 , SrTiO 3 , BaTiO 3
Transparent conductor oxides In 2 O 3 , In 2 O 3 :Sn, In 2 O 3 :F, In 2 O 3 :Zr, SnO 2 , SnO 2 :Sb, ZnO,
Semiconductor oxides ZnO:Al, Ga 2 O 3 , NiO, CoO x
Superconductor oxides YBa 2 Cu 3 O 7-x
Fluorides CaF 2 , SrF 2 , ZnF 2

How ald works

The premise behind the ALD process is a simple one. The substrate (amorphous or crystalline) is exposed to the first gaseous precursor molecule (elemental vapor or volatile compound of the element) in excess and the temperature and gas flow is adjusted so that only one monolayer of the reactant is chemisorbed onto the surface ( [link] a). The excess of the reactant, which is in the gas phase or physisorbed on the surface, is then purged out of the chamber with an inert gas pulse before exposing the substrate to the other reactant ( [link] b). The second reactant then chemisorbs and undergoes an exchange reaction with the first reactant on the substrate surface ( [link] c). This results in the formation of a solid molecular film and a gaseous side product that may then be removed with an inert gas pulse ( [link] d).

Questions & Answers

what is defense mechanism
Chinaza Reply
what is defense mechanisms
Chinaza
I'm interested in biological psychology and cognitive psychology
Tanya Reply
what does preconceived mean
sammie Reply
physiological Psychology
Nwosu Reply
How can I develope my cognitive domain
Amanyire Reply
why is communication effective
Dakolo Reply
Communication is effective because it allows individuals to share ideas, thoughts, and information with others.
effective communication can lead to improved outcomes in various settings, including personal relationships, business environments, and educational settings. By communicating effectively, individuals can negotiate effectively, solve problems collaboratively, and work towards common goals.
it starts up serve and return practice/assessments.it helps find voice talking therapy also assessments through relaxed conversation.
miss
Every time someone flushes a toilet in the apartment building, the person begins to jumb back automatically after hearing the flush, before the water temperature changes. Identify the types of learning, if it is classical conditioning identify the NS, UCS, CS and CR. If it is operant conditioning, identify the type of consequence positive reinforcement, negative reinforcement or punishment
Wekolamo Reply
please i need answer
Wekolamo
because it helps many people around the world to understand how to interact with other people and understand them well, for example at work (job).
Manix Reply
Agreed 👍 There are many parts of our brains and behaviors, we really need to get to know. Blessings for everyone and happy Sunday!
ARC
A child is a member of community not society elucidate ?
JESSY Reply
Isn't practices worldwide, be it psychology, be it science. isn't much just a false belief of control over something the mind cannot truly comprehend?
Simon Reply
compare and contrast skinner's perspective on personality development on freud
namakula Reply
Skinner skipped the whole unconscious phenomenon and rather emphasized on classical conditioning
war
explain how nature and nurture affect the development and later the productivity of an individual.
Amesalu Reply
nature is an hereditary factor while nurture is an environmental factor which constitute an individual personality. so if an individual's parent has a deviant behavior and was also brought up in an deviant environment, observation of the behavior and the inborn trait we make the individual deviant.
Samuel
I am taking this course because I am hoping that I could somehow learn more about my chosen field of interest and due to the fact that being a PsyD really ignites my passion as an individual the more I hope to learn about developing and literally explore the complexity of my critical thinking skills
Zyryn Reply
good👍
Jonathan
and having a good philosophy of the world is like a sandwich and a peanut butter 👍
Jonathan
generally amnesi how long yrs memory loss
Kelu Reply
interpersonal relationships
Abdulfatai Reply
Got questions? Join the online conversation and get instant answers!
Jobilize.com Reply

Get Jobilize Job Search Mobile App in your pocket Now!

Get it on Google Play Download on the App Store Now




Source:  OpenStax, Chemistry of electronic materials. OpenStax CNX. Aug 09, 2011 Download for free at http://cnx.org/content/col10719/1.9
Google Play and the Google Play logo are trademarks of Google Inc.

Notification Switch

Would you like to follow the 'Chemistry of electronic materials' conversation and receive update notifications?

Ask